Ceramic-on-Ceramic THA: The Good with the Bad Ceramic-on-Ceramic THA: The Good with the Bad Todd V. Swanson, MD Las Vegas, Nevada Todd V. Swanson, MD Las Vegas, Nevada Nevada Hip & Knee Center Of Excellence & Research Institute Nevada Hip & Knee Center Of Excellence & Research Institute January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices Bearing Surface Choices Head Metal Ceramic Zirconia Biolox Forte Biolox Delta Head Metal Ceramic Zirconia Biolox Forte Biolox Delta Cup Polyethylene Standard Highly cross-linked Metal Biolox Forte Biolox Delta Cup Polyethylene Standard Highly cross-linked Metal Biolox Forte Biolox Delta

Upload: dangdieu

Post on 12-Jun-2018

217 views

Category:

Documents


0 download

TRANSCRIPT

Page 1: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Ceramic-on-Ceramic THA:The Good with the Bad

Ceramic-on-Ceramic THA:The Good with the Bad

Todd V. Swanson, MDLas Vegas, Nevada

Todd V. Swanson, MDLas Vegas, Nevada

Nevada Hip & KneeCenter Of Excellence

& Research Institute

Nevada Hip & KneeCenter Of Excellence

& Research Institute

January 9, 2008 Ceramic-Ceramic 2

Bearing Surface ChoicesBearing Surface Choices

Head Metal

Ceramic• Zirconia

• Biolox Forte

• Biolox Delta

Head Metal

Ceramic• Zirconia

• Biolox Forte

• Biolox Delta

Cup Polyethylene

• Standard

• Highly cross-linked

Metal

Biolox Forte

Biolox Delta

Cup Polyethylene

• Standard

• Highly cross-linked

Metal

Biolox Forte

Biolox Delta

Page 2: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

January 9, 2008 Ceramic-Ceramic 3

Ceramic-on-Ceramic (CoC)Ceramic-on-Ceramic (CoC) Early examples

• 1969 – France (Boutin)

• 1974 – CeramTec (Germany)

• 1983-- Mittelmeier (Autophor) –U.S. (Smith & Nephew)– Failures due to:

Lack of fixation

Neck impingement

– However, minimal wear

Early examples• 1969 – France (Boutin)

• 1974 – CeramTec (Germany)

• 1983-- Mittelmeier (Autophor) –U.S. (Smith & Nephew)– Failures due to:

Lack of fixation

Neck impingement

– However, minimal wear

January 9, 2008 Ceramic-Ceramic 4

Ceramic-Ceramic Wear RatesCeramic-Ceramic Wear Rates Retrievals have shown very low wear

• >1000x less wear than conventional polyethylene

• Very favorable tribological properties– Smooth surface

– Wettable

– Hard surface

Retrievals have shown very low wear• >1000x less wear than conventional

polyethylene

• Very favorable tribological properties– Smooth surface

– Wettable

– Hard surface

Page 3: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Volumetric Wear RatesVolumetric Wear Rates

(<1000x volumetric wearthan metal-poly)

January 9, 2008 Ceramic-Ceramic 6

CoC in the USACoC in the USA 2 companies received FDA approval

Feb 3, 2003

• Wright Medical

• Stryker Orthopedics

Encore approval December 1, 2003

Several other companies followed

All ceramics produced by CeramTec

2 companies received FDA approval

Feb 3, 2003

• Wright Medical

• Stryker Orthopedics

Encore approval December 1, 2003

Several other companies followed

All ceramics produced by CeramTec

Page 4: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Concerns about CeramicsConcerns about Ceramics

Ceramic wear

Ceramic Fracture

Inability to re-use trunnion

Lack of head/liner options

Latest concern: Squeaking

Ceramic wear

Ceramic Fracture

Inability to re-use trunnion

Lack of head/liner options

Latest concern: SqueakingJanuary 9, 2008 Ceramic-Ceramic 7

January 9, 2008 Ceramic-Ceramic 8

Ceramic Fracture: Risk FactorsCeramic Fracture: Risk Factors

Poor manufacturing techniques with older components Trauma

Small head diameter

Short necks Damaged trunnion or cup

taper

Poor manufacturing techniques with older components Trauma

Small head diameter

Short necks Damaged trunnion or cup

taper

Page 5: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Cup Malposition (incorrect anteversion or vertical cup)• Microseparation/stripe wear

Sandwich type liner designs

Cup Malposition (incorrect anteversion or vertical cup)• Microseparation/stripe wear

Sandwich type liner designs

Ceramic Fracture: Risk FactorsCeramic Fracture: Risk Factors

Sandwich Design Failure Mechanisms(Park, JBJS-A, 2006)

Sandwich Design Failure Mechanisms(Park, JBJS-A, 2006)

Page 6: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Risk of fracture: 1/10,000(11 studies: 2000-2003)

Risk of fracture: 1/10,000(11 studies: 2000-2003)

(Tateiwa, Am J Orthop, 2008)(Tateiwa, Am J Orthop, 2008)

January 9, 2008 Ceramic-Ceramic 11

New Problem: SqueakingNew Problem: Squeaking

Significant squeaking in some ceramic on ceramic THA’s became apparent shortly after FDA approval of Stryker and Wright Medical hips in 2003

Significant squeaking in some ceramic on ceramic THA’s became apparent shortly after FDA approval of Stryker and Wright Medical hips in 2003

January 9, 2008 Ceramic-Ceramic 12

Page 7: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Proposed CausesProposed Causes Impingement Ligament laxity /

microseparation / stripe wear Inadequate lubrication Particulate metal

debris New “beta” titanium

alloy (TMFZ)

Impingement Ligament laxity /

microseparation / stripe wear Inadequate lubrication Particulate metal

debris New “beta” titanium

alloy (TMFZ)January 9, 2008 Ceramic-Ceramic 13

1 Common Denominator1 Common Denominator

Almost all studies with large numbers of squeaky ceramic hips are Stryker Trident cups mated with Stryker Accolade Stems

Almost all studies with large numbers of squeaky ceramic hips are Stryker Trident cups mated with Stryker Accolade Stems

January 9, 2008 Ceramic-Ceramic 14

Page 8: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Stryker Trident cupStryker Trident cup

Ceramic encased in metal shell which extends past ceramic face

Ceramic encased in metal shell which extends past ceramic face

Overhanging rim increases risk for impingement

Overhanging rim increases risk for impingement

January 9, 2008 Ceramic-Ceramic 16

Page 9: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Stryker Accolade StemStryker Accolade Stem

TMZF beta titanium allow (25% greater flexibility than Ti-6Al-4V)• Titanium• Molybdenum• Zirconium• Iron

HA Coated

TMZF beta titanium allow (25% greater flexibility than Ti-6Al-4V)• Titanium• Molybdenum• Zirconium• Iron

HA Coated

Stryker CoC IDE StudyStryker CoC IDE Study 4 study arms:

• 380 CoC vs 95 controls

• All used Omnifit stem (Ti-6Al-4V)

4 study arms:• 380 CoC vs 95 controls

• All used Omnifit stem (Ti-6Al-4V)

January 9, 2008 Ceramic-Ceramic 18

Page 10: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

1st & 2nd arms used ABC cup (194)

3rd arm used metal on poly control

4th arm used Trident cup (186)

1st & 2nd arms used ABC cup (194)

3rd arm used metal on poly control

4th arm used Trident cup (186)

January 9, 2008 Ceramic-Ceramic 19

Stryker IDE StudyStryker IDE StudyOnly 0.8% incidence of

transient squeaking after 8 year F/U(Capello, J Arth, 2008)

Only 0.8% incidence of transient squeaking after 8 year F/U(Capello, J Arth, 2008)

Page 11: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Murphy, CCJR, Orlando, FL, 12/08Murphy, CCJR, Orlando, FL, 12/08

1100 CoC THA’s with flush mounted ceramic liners-1 squeaker

Of the Trident cups, only those mated with Accolade stem squeaked!

1100 CoC THA’s with flush mounted ceramic liners-1 squeaker

Of the Trident cups, only those mated with Accolade stem squeaked!

January 9, 2008 Ceramic-Ceramic 21

Squeaky Trident CupsSqueaky Trident Cups

January 9, 2008 Ceramic-Ceramic 22

Page 12: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

My ResultsMy Results

314 CoC hips performed 1999-2006

5 brands of hips implanted

276 Contacted telephonically for questions re: squeaking

Cup positions compared radiographically

314 CoC hips performed 1999-2006

5 brands of hips implanted

276 Contacted telephonically for questions re: squeaking

Cup positions compared radiographically

January 9, 2008 Ceramic-Ceramic 23

Brands ImplantedBrands Implanted

156 Encore Keramos

67 Plus MPF

50 Stryker Trident (all with Accolade stems)

34 Wright Medical Lineage

7 Smith & Nephew Reflection

156 Encore Keramos

67 Plus MPF

50 Stryker Trident (all with Accolade stems)

34 Wright Medical Lineage

7 Smith & Nephew ReflectionJanuary 9, 2008 Ceramic-Ceramic 24

Page 13: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

DemographicsDemographics

Total Hips: 314Total Patients: 270Males : Females =146 : 124Left : Right = 158 : 156Bilaterals: 44 Mean Age: 47.2±8.3Mean BMI: 28.1±6.9

Total Hips: 314Total Patients: 270Males : Females =146 : 124Left : Right = 158 : 156Bilaterals: 44 Mean Age: 47.2±8.3Mean BMI: 28.1±6.9

January 9, 2008 Ceramic-Ceramic 25

DiagnosesDiagnoses

DJD-190AVN-44DDH-21Post Traumatic-16RA-15Perthes-14Other-14

DJD-190AVN-44DDH-21Post Traumatic-16RA-15Perthes-14Other-14

Page 14: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

ResultsResultsMean F/U: 52 months (24-110) 20 (7.2%) hips with ANY reported

squeaking• 15/45 Stryker (33.3%) • 1/29 Wright Medical (3.4%)• 3/143 Encore (2.1%)• 1/52 Plus (1.4%)

Mean onset to squeaking: 16±13 months

Mean F/U: 52 months (24-110) 20 (7.2%) hips with ANY reported

squeaking• 15/45 Stryker (33.3%) • 1/29 Wright Medical (3.4%)• 3/143 Encore (2.1%)• 1/52 Plus (1.4%)

Mean onset to squeaking: 16±13 months

January 9, 2008 Ceramic-Ceramic 27

Squeaking FrequencySqueaking FrequencyStryker Encore Plus Wright

Daily 3 0 0 04-5/week 2 0 0 01-2/week 1 2 1 0

Rare 8 1 0 0NA 1 0 0 1

TOTAL 15 3 1 1

Page 15: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Squeaking IntensitySqueaking IntensityStryker Encore Plus Wright

Creates Social Problem 2 0 0 0Always

Perceptible 5 0 0 0Occ Perceptible

to Others 5 1 1 0Perceptible

Only to Patient 2 2 0 0NA 1 0 0 1

TOTAL 15 3 1 1

Problem SqueakingProblem Squeaking

Frequency >1/wk

Stryker 6 13.3%

Encore 2 1.4%

Plus 1 1.9%

Perceptible to Others

Stryker 12 26.7%

Encore 1 0.7%

Plus 1 1.9%

Page 16: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

Squeakers vs Non-SqueakersSqueakers vs Non-Squeakers

No difference in:• Demographics

• Cup size or position

• Head size

• Stem Offset

• Neck length

No difference in:• Demographics

• Cup size or position

• Head size

• Stem Offset

• Neck length

January 9, 2008 Ceramic-Ceramic 31

ConclusionConclusion

Something related to elevated rim ceramic inlay (Trident) and TMFZ beta titanium allow (Accolade) leads to an unusually high incidence of squeaking

Something related to elevated rim ceramic inlay (Trident) and TMFZ beta titanium allow (Accolade) leads to an unusually high incidence of squeaking

January 9, 2008 Ceramic-Ceramic 32

Page 17: Ceramic on Ceramic--the Good with the Bad - Mini … THA: The Good with the Bad ... January 9, 2008 Ceramic-Ceramic 2 Bearing Surface Choices ... Ceramic on Ceramic--the Good with

January 9, 2008 Ceramic-Ceramic 33

SummarySummary Ceramic on Ceramic THA is a reliable,

durable articulation provided certain precautions are followed:

Avoid cup malposition: vertical placement or inaccurate version

Avoid use in overly lax soft tissues

Avoid small heads, short necks

Avoid elevated rim liners (Stryker Trident cups) with TMFZ stems (Stryker Accolade) to avoid squeaking

Ceramic on Ceramic THA is a reliable, durable articulation provided certain precautions are followed:

Avoid cup malposition: vertical placement or inaccurate version

Avoid use in overly lax soft tissues

Avoid small heads, short necks

Avoid elevated rim liners (Stryker Trident cups) with TMFZ stems (Stryker Accolade) to avoid squeaking

January 9, 2008 Ceramic-CeramicCeramic-Ceramic 34

Thank-YouThank-You

Todd V. Swanson, MDLas Vegas, Nevada

Todd V. Swanson, MDLas Vegas, Nevada

Nevada Hip & KneeCenter Of Excellence

& Research Institute

Nevada Hip & KneeCenter Of Excellence

& Research Institute