Coating Systems Maritime & Offshore Are you searching for the ideal corrosion protection? Just give us a call! +49 (0) 52 23 - 96 276-0 Phone: +49 (0)5223 – 96 276-0 | Fax: +49 (0)5223 – 96 276-17 | eMail: [email protected] | Web: www.ceramic-polymer.de Ceramic Polymer GmbH | Daimlerring 9 | D-32289 Roedinghausen

Upload: doannhi

Post on 21-May-2018

222 views

Category:

Documents


2 download

TRANSCRIPT

Page 1: Ceramic Polymer GmbH | Daimlerring 9 | D-32289 … · water tanks NORSOK M-501 rev. 3, system approvals 1, 3 B u. 7 Germanischer Lloyd – ballast water tanks + offshore windmills

Coating Systems Maritime & Offshore

Are you searching for the ideal corrosion protection?

Just give us a call!+49 (0) 52 23 - 96 276-0

Phone: +49 (0)5223 – 96 276-0 | Fax: +49 (0)5223 – 96 276-17 | eMail: [email protected] | Web: www.ceramic-polymer.de

Ceramic Polymer GmbH | Daimlerring 9 | D-32289 Roedinghausen

Page 2: Ceramic Polymer GmbH | Daimlerring 9 | D-32289 … · water tanks NORSOK M-501 rev. 3, system approvals 1, 3 B u. 7 Germanischer Lloyd – ballast water tanks + offshore windmills

Maritime Constructions & Offshore Facilities Internal External

Coating System No. MI-1 MI-2 MI-3 MI-4 MI-5 MI-6 MI-7 ME-1 ME-2

Products CK-54 SF CK-54 SF ARAMCO–approved APCS-2i

PROGUARD CN100

PROGUARD CN100iso

PROGUARD CN200

PROGUARD CN-1M

PROGUARD M CK-STP PROGUARD 169(optional for UV-stability)

temperature resistance wet 80° Cdry 90° C

wet 130° Cdry 150° C

wet 120° Cdry 140° C

wet 140° Cdry 170° C

wet 130° C dry 150° C

wet 130° Cdry 150° C

wet 70° Cdry 90° C 120°C 120°C

optionally implemented mechanism against bio corrosion (pitting corrosion) induced by SRB-bacteria – patented ✔ ✔ ✔ ✔

optional antistatic property ✔ ✔ ✔ ✔

abrasion resistance (ASTM D4060) 60 mg 80 mg 80 mg 80 mg 80 mg 60 mg 28 mg 100 mg 80 mg

drinking water & food safety up to 40° C up to 85° C

DFT depending on viscosity 400-1.000 µm 300-1.000 µm 300-1.000 µm 400-1.000 µm 300-1.000 µm 400-1.000 µm 300 µm 1-2 x 100-150 µm 50-60 µm

volume solids, depending on version 100% 100% 97-100% 97-100% 97-100% 97-100% 84% 57-75% 55-65%

cathodic disbonding test(ASTM G42 + G8) ✔ ✔ ✔ ✔ ✔ ✔

autoclave test with explosive decompression(natural gas, 100 bar, 100° C) ✔ ✔ ✔ ✔ ✔

salt spray test (h)(DIN EN ISO 9227:2006-10) 10.000 10.000 8.000 8.000 10.000 10.000 6.000 3.000

more tests and certificatesGermanischer Lloyd- ballast

water tanks NORSOK M-501 rev. 3,system approvals 1, 3 B u. 7

Germanischer Lloyd – ballast water tanks +

offshore windmills

acids, alkaline solutions, (pH 5-11), brine, oils, CO2, H2S, Hg, HgS <= 60°C ✔ ✔ ✔ ✔ ✔ ✔ ✔ ✔

acids, alkaline solutions, (pH 4-10), brine, oils, CO2, H2S, Hg, HgS <= 80°C ✔ ✔ ✔ ✔ ✔ ✔ ✔

acids, alkanline solutions, (pH 4-10), brine, oils, CO2, H2S, Hg, HgS <=110°C ✔ ✔ ✔ ✔

test E85 – ethyl alcohol, methyl alcohol/petrol, add-blue-solutions, RME ✔ ✔ ✔ ✔

resistance against methyl alcohol ✔ ✔ ✔ ✔

deionized water(long-term test, 1 year constantly at 50°C) ✔ ✔ ✔ ✔

98% H2SO4 / pure methyl alcohol / 3% NaCl-solution>5.000 h, (1/3 / 1/3 / 1/3 at 50°C) ✔

chem

ical r

esist

ance

phys

ical p

rope

rtie

s

= wet / liquid storage media = dry / vapors or gases, external influences

Ceramic Polymer Coating Systems

The mentioned layer thicknesses are just guidelines. Please contact our product consultants, they provide you a precise proposal. Stand 02/2011