Download - 3 d ripple print
What is “3-D Ripple Print”?3-dimensional transparent print or
Special embossed color print on cellulosic goods
Exclusive recipe by “Permafin-PN..” systemPrimarily for cellulosic goodsUnique and exceptional printFully creative finish
1. Additives for Transparent & Ripple PrintPermafin-PB-37, Permafin-PN-01Permafin-RPP, Permafin-PN-119Crosslinker-UX, Microderm-SKCAquarepel-XC/Conc, Aquarepel-EX-001MTriplex-PTF, Altraplex-AW
2. Recipe for Transparent and Ripple printi) Roller Print [mangle padding] – for wovenii) Rotary print – for woveniii) Rotary print – for knit
Specification Additives
Item Composition Appearance pH [10%]
Ionicity Solubility [in water]
Permafin-PN-01Permafin-PN-37Permafin-PN-119
Special urethane resins for ripple print [soft handle]
Colorless to slightly yellowish viscous liquid
7 ± 15.5 ± 15.5 ± 1
NonionNonionNonion
Easily soluble at cold or warm water
Permafin-RPP Special urethane resins for ripple print [stiff handle]
Light beige viscous liquid
5 ± 1 Nonion Easily soluble at cold or warm water
Crosslinker-UX Catalyst of Urethane resins
Light beige viscous liquid
5 ± 1 Nonion Easily soluble
Aquarepel-FC-1500
Fluoro polyacrylate White to yellowish liquid 2.5 ± 0.5
Cation Easily soluble
Aquarepel-EX-001M
Blocked polyisocyanate
Light beige Dispersion
7 ± 1 Nonion Easily soluble
Altraplex- AW Organic phosphoric compound
Light yellowish clear liquid 9 ± 1 Weak anion
Easily soluble
Microderm-SKC
Special silicone copolymer
Milky white liquid 4.5 ± 1 Nonion Easily soluble
Triplex-PTF Special polymer Off white liquid > 5 Anion Soluble
Permafin- PN-37Permafin- PN-01Permafin- PN 119Urethane resin for transparent print and color printExcellent alkaline stability. No hydrolysis problemPrevent staining of dyes in washing processGood transparency and vivid print on goodsFilm with soft handle [PN 119*>PN 37 > PN-01]Permafin- PN 119 provides more volume
Additives
Permafin- RPP
Urethane resin for transparent print and color printExcellent alkaline stability. No hydrolysis problemPrevent staining of dyes in washing processGood transparency and vivid print on goodsGood volume feeling to the clothes and bed clothesFilm with medium to stiff handle
Additives
CROSSLINKER-UXCatalyst for urethane resinPromotes activation and fixation of Urethane resinApplying quantity: 5 ~ 10% of urethane resin appliedMICRODERM-SKCSpecific softener for Ripple print [only for knit]Form film by itself without any bad influence on printApplying quantity: 30 ~ 50 g/l
Additives
AQUAREPEL-FC 1500Film protector for color Ripple print [by reactive dyes]Prevent color change/lost of dyes under strong alkalis
Aquarepel-EX-001MCatalyst of FC 1500 in color ripple printPrevent drape property of fabricsApplying quantity: ca. 20% of FC 1500 applied
Additives
Altraplex- AWUsed in washing process after alkali ageing of Ripple PrintPrevent yellowing of transparent print film after dryingWhen neutralizing by Acid, used jointly in a bathApplying quantity: 3~5 g/l
AdditivesTriplex-PTFThickener for viscosity controlApplying quantity: x% [for viscosity ca. 5000 cps
1. Roller Print for WovenRecipe:Permafin--RPP : 95%Crosslinker-UX : 5%Thickener [Triplex-PTF] : x% [ca. 5000 cps of viscosity]** If softer handle is required, increase the quantity of Permafin- PN-01 [or PN 37, PN 119, Microderm-SKC] while reducing the quantity of Permafin--RPPPrint condition: Mangle padding [Roller Print] Setting [190ºC x 100 yd/mm] Alkali treatment [98% NaOH 32º ~ 35º Be] Rinsing & neutralizing Tentering [170ºC x 70 yd/min]
Application
2. Rotary print for wovenRecipe:Permafin- PN-01 : 70% [or Permafin- PN 37, PN 119]Permafin- RPP : 25%Crosslinker-UX : 5%Thickener [Triplex-PTF] : X% [ca. 5000 cps of viscosity]
Print condition:Printing Curing [180ºC x 2 min] Padding [98% NaOH 320 ~ 350 g/l] Rinsing & neutralizing Tentering [180ºC x 90 sec]
Application
3. Rotary print for knit:Recipe:Permafin- PN-01 : 55% [or Permafin- PN 37, PN 119]Permafin- RPP : 25%Crosslinker-UX : 5%Microderm- SKC : 15%Thickener [Triplex-PTF] : X% [ca. 5000 cps for viscosity]
Print condition:Pre-treatment Printing Curing [180ºC x 2 min] Padding [98% NaOH, 320~350 g/l] Rinsing & neutralizing tentering [180ºC x 1 min 30 sec]
Application