CAREER: Synthesis, Microstructure, and Mechanical Behavior of Metallic Thin Films with Nanoscale Growth Twins Xinghang Zhang, Texas Engineering Experiment Station, DMR 0644835. Explore dislocation - twin boundary interaction via in situ nanoindentation in TEM - PowerPoint PPT PresentationTRANSCRIPT
![Page 1: Explore dislocation - twin boundary interaction via in situ nanoindentation in TEM](https://reader034.vdocument.in/reader034/viewer/2022050721/56814f63550346895dbd177b/html5/thumbnails/1.jpg)
CAREER: Synthesis, Microstructure, and Mechanical Behavior of Metallic Thin Films with Nanoscale Growth Twins
Xinghang Zhang, Texas Engineering Experiment Station, DMR 0644835
• Explore dislocation - twin boundary interaction via in situ nanoindentation in TEM
• Investigate nanotwins in Ag filmsWork hardening of nanotwinned Cu
Script Mater, Acta Mater. 2011.
Epitaxial nanotwinned Ag films
Acta Mater., 2011.
Multiplication of dislocation at twin boundary in nanotwinned Cu
![Page 2: Explore dislocation - twin boundary interaction via in situ nanoindentation in TEM](https://reader034.vdocument.in/reader034/viewer/2022050721/56814f63550346895dbd177b/html5/thumbnails/2.jpg)
EducationOsman Anderoglu (Ph.D. in 09). Now a postdoctor at Los Alamos.
Nan Li (Ph.D. in 2010). A postdoctor at Los Alamos
Nan Li won the Acta Mater. Student paper contest award, 2011.
Dan Bufford (Ph.D. candidate). NSF IGERT Fellow, Work on nanotwinned Ag films.
Yue Liu (defended MS. in 2010). Continue for Ph.D. to work on in situ nanoindentation.
Broader impact
• Hosted 2 minority summer undergraduate students (Matai Wilson, and Cassandra Lee Gutierrez) to work on nanoindentation, TEM sample preparations. • Collaborate with A. Misra et al through
CINT • Journal articles: 3 in Acta Mater., 1 in
Scripta Mater. (10-11)
• Numerous presentations at TMS, and MRS.
• Invited talks at Zhejiang University and Hefei University of Technology
• Adjunct professor at Hefei University of Technology
CAREER: Synthesis, Microstructure, and Mechanical Behavior of Metallic Thin Films with Nanoscale Growth Twins
Xinghang Zhang, Texas Engineering Experiment Station, DMR 0644835