low temperature and high temperature processing eva film for laminating glass

1
Guangzhou Huichi Glass Technical Co.,ltd 2 nd Floor West, Building No.A27,Huifu Industrial Zone,Tianxin Village, Xicha Road,Guangzhou,China Tel:+86 20-3649 9996 Fax :+86 20-3649 2206 www.huichiglass.com contact: [email protected] Low temperature and high temperature processing EVA film 1. High transparency: light transmittance 92.1%, Haze 0.3% 2. Wide range of adhesion: processing temperature between 80-130provide good adhesive strength 3. Excellent UV blocking, to resist 99% UV, ensuring the safety of indoor environment. 4. Mobility, easy to fill in concave space, ideal choice for fabric and other insertion materials. For this kind of EVA film, it can process at 80 degree for decorative fabric/paper laminating, especially for the PDLC film laminating. Below is the processing data for the smart switchable glass laminating. But if you want to laminate the high transparency safety glass, you can process it at 135 degree.

Upload: guangzhou-huichi-glass-technical-company

Post on 21-Jul-2015

40 views

Category:

Design


0 download

TRANSCRIPT

Page 1: Low temperature and high temperature processing EVA film for laminating glass

Guangzhou Huichi Glass Technical Co.,ltd2nd Floor West, Building No.A27,Huifu Industrial Zone,Tianxin Village,

Xicha Road,Guangzhou,ChinaTel:+86 20-3649 9996 Fax :+86 20-3649 2206

www.huichiglass.com contact: [email protected] temperature and high temperature processing EVA film

1. High transparency: light transmittance >92.1%, Haze <0.3%

2. Wide range of adhesion: processing temperature between 80-130℃ provide good adhesive strength

3. Excellent UV blocking, to resist 99% UV, ensuring the safety of indoor environment.

4. Mobility, easy to fill in concave space, ideal choice for fabric and other insertion materials.

For this kind of EVA film, it can process at 80 degree for decorative fabric/paper laminating, especially for the PDLC film laminating.Below is the processing data for the smart switchable glass laminating.

But if you want to laminate the high transparency safety glass, you can process it at 135 degree.