Information Sheet
Reconstitution Procedure
Materials
Opadry II film coating system.
Water, deionized or distilled preferred, ambient
temperature (maximum 30 C)
Equipment Variable-speed mixer capable of producing and
maintaining a vortex.
Propeller stirrer. For optimum mixing, utilize a propeller
with a diameter equivalent to 1/4 - 1/3 of the diameter
of the mixing vessel. (see Figure 1.)
Mixing vessel large enough to contain a liquid volume
15% to 25% greater than the total suspension being
prepared. The liquid height and vessel diameter should
be equal.
*Mixing Procedure1. Weigh necessary quantity of Opadry II film coating
system.
2. Weigh necessary quantity of water into the mixing vessel.
3. With the propeller in the center and as close to the bottom
of the vessel as possible, stir the water to form a vortex
without drawing air into the liquid.
4. Steadily add the Opadry II system powder to the vortex,
avoiding powder flotation on the liquid surface. If
required, increase the stirrer speed in order to maintain
the vortex .
5. After all the Opadry II system has been added, reducethe mixer speed to nearly eliminate the vortex. Mix for
45 minutes.
OPADRY II film coating systems are quick and easy to prepare. Simply add OPADRY II film coating
system powder to water and mix for 45 minutes with a propeller stirrer.*
The coating suspension can be made with up to 20% solids. Your Area Technical Manager can recommend
the ideal solids for your specific Opadry II system and your equipment.
Suspension Handling
The prepared Opadry II dispersion can be
pumped directly from the preparation vessel if
desired.
We recommend that the Opadry II dispersion be
gently agitated during the coating process.
Figure 1.
-
7/27/2019 Opadry II Reconstitution 0
2/2
Opadry II is a trademark of BPSI Holding, Inc.
FC/OPADRYIIRECON/06/99 REV.2_0703
World Headquarters
Colorcon
415 Moyer Blvd., P.O. Box 24, West Point, PA 19486-0024
Tel: 215-699-7733 Fax: 215-661-2605 Web Site @http://www.colorcon.com
Locations Telephone Facsimile
Asia /Pac ifi c
Singapore 65-6438-0318 65-6438-0178
Fuji-gun, Shizuoka, Japan 81-5-4465-2711 81-5-4465-2730
Shanghai, China 86-21-5442-2222 86-21-5442-2229
Goa, India 91-0832-2883434 91-0832-2883440
Seoul, Korea 822-2057-2173 822-2057-2179
Latin America
Buenos A ires,Argentina 5 4-9- 11- 4552- 1565 54- 11- 9-45 52-39 97
Cotia, Brasil 55-11-4612-4262 55-11-4612-3307
Bogota, Colombia 571-418-1202 571-418-1257
Caracas, Venezuela 58-212-793-3459 58-212-781-2619
Santa Fe, Mexico 52-55-5292-1611 52-55-5292-1750
Locations Telephone Facsimile
United States
Santa Ana, California 714-549-0631 714-549-4921
Indianapolis,lndiana 317-545-6211 317-545-6218
Humacao, Puerto Rico 787-852-3815 787-852-0030
Europe
Dartford, Kent, England 44-1322-293000 44-1322-627200
Bougival, France 33-1-3082-1582 33-1-3082-7879
Idstein, Germany 49-6126-9961-0 49-6126-9961-11
Gallarate, Italy 39-0331-776932 39-0331-776831
Budapest, Hungary 36-1-200-8000 36-1-200-8010
Istanbul, Turkey 90-216-465-0360 90-216-465-0361
Barcelona, Spain 34-9-3589-3756 34-9-3589-3792
The information contained herein, to the best of our knowledge is true and accurate. Any recommendations or suggestions are made without warranty or guarantee, since the
conditions of use are beyond our control. Any information contained herein is intended as a recommendation for use of our products so as not to infringe on any patent.
2003 Colorcon. The information contained in this document is proprietary to Colorcon and may not be used or disseminated inappropriately.