welding procedure specification (wps) of the manufacturer
TRANSCRIPT
![Page 1: Welding Procedure Specification (WPS) of the Manufacturer](https://reader035.vdocument.in/reader035/viewer/2022081816/552dc9364a795906588b47d3/html5/thumbnails/1.jpg)
Welding Procedure Specification (WPS) of the Manufacturer
Page 1 of 9
Dokument4 Z449DE / 2003-04/IP
Company: Address:
Phone no.: Fax no.:
E-mail:
Telex no.:
Responsible welding supervisor: Work/Work's division:
Address:
Welding procedure specification (WPS)
WPS-No.: Date: Test report (WPAR) no: Rev. no.: Welding process: Welding position(s): Parent material(s) spec.: Joint type: Material thickness [mm]: Outside diameter [mm]: Method of preparation and cleaning:
Joint preparation details (sketch) Joint design Welding sequences
Welding details Run Process Size of filler
metal Current
[A]
Voltage
[V]
Type of current / polarity
Wire feed speed
Travel speed *
[cm/min]
Heat input *
[J/cm]
Filler metal
Manufacturer: Brand name:
![Page 2: Welding Procedure Specification (WPS) of the Manufacturer](https://reader035.vdocument.in/reader035/viewer/2022081816/552dc9364a795906588b47d3/html5/thumbnails/2.jpg)
Welding Procedure Specification (WPS) of the Manufacturer
Page 2 of 9
Dokument4 Z449DE / 2003-04/IP
Quality grade: Classification: Any special baking or drying:
Gas
Shielding: Gas flow rate: Backing: Gas flow rate:
Flux
Manufacturer: Brand name: Classification: Any special baking or drying:
Tungsten electrode type/∅: Gouging/grinding: Preheating temperature: Interpass temperature:
Post weld heat treatment and / or aging *
Time, temperature, method: Heating and cooling rate:
Other information, e. g.*
Weaving (max. width of run): Oscillation (amp, freq.,dwell time): Pulse welding details: Stand-off distance: Plasma welding details: Torch angle:
Welding over shop primer *
Brand name: Dry film thickness: Other:
Place/Date Stamp Signature of Manufacturer’s Welding Supervisor * If required
![Page 3: Welding Procedure Specification (WPS) of the Manufacturer](https://reader035.vdocument.in/reader035/viewer/2022081816/552dc9364a795906588b47d3/html5/thumbnails/3.jpg)
Welding Procedure Test / Production Test
Page 3 of 9
Dokument4 Z449DE / 2003-04/IP
Details relating to test welds: WPS-No.
Company: Address:
Phone no.: Fax no.:
E-mail:
Telex no.:
Responsible welding supervisor: Work/Work's division:
Address:
Welding procedure specification (pWPS)
pWPS-No.: Date of test: Test report (WPAR) no: Rev. no.: Examiner or test body: Welder's name: Welding process: Welding position(s): Parent material(s) spec.: Joint type: Material thickness [mm]: Outside diameter [mm]: Method of preparation and cleaning:
Joint preparation details (sketch) Joint design Welding sequences
Welding details Run Process Size of filler
metal Current
[A]
Voltage
[V]
Type of current / polarity
Wire feed speed
Travel speed *
[cm/min]
Heat input *
[J/cm]
![Page 4: Welding Procedure Specification (WPS) of the Manufacturer](https://reader035.vdocument.in/reader035/viewer/2022081816/552dc9364a795906588b47d3/html5/thumbnails/4.jpg)
Welding Procedure Test / Production Test
Page 4 of 9
Dokument4 Z449DE / 2003-04/IP
Filler metal
Manufacturer: Brand name: Quality grade: Classification: Any special baking or drying:
Gas
Shielding: Gas flow rate: Backing: Gas flow rate:
Flux
Manufacturer: Brand name: Classification: Any special baking or drying:
Tungsten electrode type/∅: Gouging/grinding: Preheating temperature: Interpass temperature:
Post weld heat treatment and / or aging *
Time, temperature, method: Heating and cooling rate:
Other information, e. g. *
Weaving (max. width of run): Oscillation (amp, freq.,dwell time): Pulse welding details: Stand-off distance: Plasma welding details: Torch angle:
Welding over shop primer *
Brand name: Dry film thickness: Other:
![Page 5: Welding Procedure Specification (WPS) of the Manufacturer](https://reader035.vdocument.in/reader035/viewer/2022081816/552dc9364a795906588b47d3/html5/thumbnails/5.jpg)
Welding Procedure Test / Production Test
Page 5 of 9
Dokument4 Z449DE / 2003-04/IP
We hereby confirm that the specimen welds have been prepared and performed satisfactorily using the data listed above, in accordance with the Rules for Welding issued by Germanischer Lloyd.
Place/Date Stamp Signature of Manufacturers Welding Supervisor
Place/Date Stamp Signature of Society Surveyor * If required
![Page 6: Welding Procedure Specification (WPS) of the Manufacturer](https://reader035.vdocument.in/reader035/viewer/2022081816/552dc9364a795906588b47d3/html5/thumbnails/6.jpg)
Welding Procedure Test / Production Test
Page 6 of 9
Dokument4 Z449DE / 2003-04/IP
Test results: WPS-No.
Company:
Examiner or test body: Test report (WPAR) no: Welding proced. spec.(WPS): (WPS):
Non-destructive testing Test method Results Test report no.
Visual inspection: Radiographic test:
Ultrasonic test: Magnetic particle test:
Dye penetrate test:
-test:
Tensile tests **
Standard:
Speci-men,
form/no.
Dimension mm
Cross-section
[mm²]
Test load Fr
[N]
Yield or 0,2% proof
stress [N/mm²]
Breaking load Fm [N]
Tensile strength
Rm [N/mm²]
Elongation (L0 = mm)
[%]
Reduction in area
[%]
Position of fracture, remarks
Require-ments
Bend tests **
Standard:
Speci-men,
form/no.
Dimensions
[mm]
Bending mandrel diameter
[mm]
Bending angel
[degrees]
Elongation on bending (L0 = mm)
[%]
Position of fracture, remarks
Require-ments
![Page 7: Welding Procedure Specification (WPS) of the Manufacturer](https://reader035.vdocument.in/reader035/viewer/2022081816/552dc9364a795906588b47d3/html5/thumbnails/7.jpg)
Welding Procedure Test / Production Test
Page 7 of 9
Dokument4 Z449DE / 2003-04/IP
Speci-men,
form/no.
Dimensions
[mm]
Bending mandrel diameter
[mm]
Bending angel
[degrees]
Elongation on bending (L0 = mm)
[%]
Position of fracture, remarks
Notched bar impact tests **
Standard: Shape of specimen: Sizes: Specimen, no., pos. of
notch
Test temp.
[°C]
Individual values
[J]
Average value
[J]
Position of fracture, remarks
1 2 3 min min Require-
ments
Hardness tests **
Standard: Type, test load:
Position of measurement (sketch/diagram)
![Page 8: Welding Procedure Specification (WPS) of the Manufacturer](https://reader035.vdocument.in/reader035/viewer/2022081816/552dc9364a795906588b47d3/html5/thumbnails/8.jpg)
Welding Procedure Test / Production Test
Page 8 of 9
Dokument4 Z449DE / 2003-04/IP
Fracture test
Standard:
Butt weld Fillet weld Position of fracture:
Results:
Metallographic examinations **
Standard: Results: (if necessary, attach photographs/explanations on a separate sheet)
Other tests **
Standard: Type:
Results:
![Page 9: Welding Procedure Specification (WPS) of the Manufacturer](https://reader035.vdocument.in/reader035/viewer/2022081816/552dc9364a795906588b47d3/html5/thumbnails/9.jpg)
Welding Procedure Test / Production Test
Page 9 of 9
Dokument4 Z449DE / 2003-04/IP
The trial welds and mechanical-technological tests have been carried out under supervision of the Surveyor of Germanischer Lloyd.
Place/Date Stamp Signature of Welding Supervisor
Place/Date Stamp Signature of Examiner or Test body
Place/Date Stamp Signature of Society Surveyor
Remark: The final assessment of the results and the certification of the welding procedure test will be performed by the Head Office Hamburg, Division NCM.
* If required ** The laboratory test records are enclosed to this test report.