Atomic Layer Depositionfor Microchannel Plates
Jeffrey Elam
Argonne National Laboratory
September 24, 2009
![Page 2: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009](https://reader036.vdocument.in/reader036/viewer/2022062805/5697c0031a28abf838cc3db2/html5/thumbnails/2.jpg)
Atomic Layer Deposition (ALD)
Layer-by-layer thin film coating method Atomic level control over thickness and composition Precise coatings on 3-D objects Deposit nearly any material (oxides, nitrides, metals, etc.)
Example:ALD Zinc Oxide in
deep trenches
![Page 3: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009](https://reader036.vdocument.in/reader036/viewer/2022062805/5697c0031a28abf838cc3db2/html5/thumbnails/3.jpg)
Large Area Photodetector
Microchannel Plate (MCP)
– Electron amplifier (x104-107)
3
![Page 4: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009](https://reader036.vdocument.in/reader036/viewer/2022062805/5697c0031a28abf838cc3db2/html5/thumbnails/4.jpg)
Microchannel Plates (MCPs)
Conventional Fabrication:– Draw glass fiber bundle– Slice and polish– Chemical etch, heat in hydrogen
Problems:– Expensive– Resistance and secondary emission properties are linked– Long conditioning process needed– Thermal runaway
4
![Page 5: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009](https://reader036.vdocument.in/reader036/viewer/2022062805/5697c0031a28abf838cc3db2/html5/thumbnails/5.jpg)
ALD for Fabrication of MCPs
Start with porous, insulating substrate
– Glass capillary plate
– Anodic aluminum oxide (AAO) membrane ALD of resistive film on all surfaces (inside of pores, on faces, etc.) ALD of secondary electron emissive film Deposit metal electrodes on outer surfaces
5
33 mm
![Page 6: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009](https://reader036.vdocument.in/reader036/viewer/2022062805/5697c0031a28abf838cc3db2/html5/thumbnails/6.jpg)
MCP Structure
6
1) resistive coating (ALD)2) emissive coating (ALD)3) conductive coating (thermal
evaporation or sputtering)
pore
![Page 7: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009](https://reader036.vdocument.in/reader036/viewer/2022062805/5697c0031a28abf838cc3db2/html5/thumbnails/7.jpg)
ALD for Resistive Coating
Target: 10-100 MΩ through MCP ZnO: conductor Al2O3: insulator
ZnO/ Al2O3 alloy – tunable resistivity
Tune composition and thickness of film to adjust MCP resistance
7
![Page 8: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009](https://reader036.vdocument.in/reader036/viewer/2022062805/5697c0031a28abf838cc3db2/html5/thumbnails/8.jpg)
ALD for Emissive Coating
8
Many material possibilities Tune SEE along pore
SiO2Al2O3
MgO
ZnO
![Page 9: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009](https://reader036.vdocument.in/reader036/viewer/2022062805/5697c0031a28abf838cc3db2/html5/thumbnails/9.jpg)
Cross-Sectional Elemental Maps of ALD MCP
9
Zn
SEM Si
Al Au
ALD ZnO and Al2O3 extend into pores
Sputtered Au only on edge of pores
Glass capillary plate ALD ZnO/Al2O3
Sputter gold electrodes
![Page 10: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009](https://reader036.vdocument.in/reader036/viewer/2022062805/5697c0031a28abf838cc3db2/html5/thumbnails/10.jpg)
Cross-Sectional Image of ALD Film in MCP
10
ALD Film
100 nm ALD film visible in middle of MCP
Glass
![Page 11: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009](https://reader036.vdocument.in/reader036/viewer/2022062805/5697c0031a28abf838cc3db2/html5/thumbnails/11.jpg)
Questions?
11